Modification of nanocellulose films in deep eutectic solvents using vinyl esters
Lakovaara, Matias; Sirviö, Juho Antti; Sliz, Rafal; Vida, Július; Homola, Tomáš; Liimatainen, Henrikki (2022-09-14)
Lakovaara, M., Sirviö, J.A., Sliz, R. et al. Modification of nanocellulose films in deep eutectic solvents using vinyl esters. Cellulose 29, 9073–9087 (2022). https://doi.org/10.1007/s10570-022-04840-y
© The Author(s) 2022. This article is licensed under a Creative Commons Attribution 4.0 International License, which permits use, sharing, adaptation, distribution and reproduction in any medium or format, as long as you give appropriate credit to the original author(s) and the source, provide a link to the Creative Commons licence, and indicate if changes were made. The images or other third party material in this article are included in the article's Creative Commons licence, unless indicated otherwise in a credit line to the material. If material is not included in the article's Creative Commons licence and your intended use is not permitted by statutory regulation or exceeds the permitted use, you will need to obtain permission directly from the copyright holder. To view a copy of this licence, visit http://creativecommons.org/licenses/by/4.0/.
https://creativecommons.org/licenses/by/4.0/
https://urn.fi/URN:NBN:fi-fe2023052547970
Tiivistelmä
Abstract
The hydrophilicity of nanocellulose materials mitigates their good mechanical and oxygen barrier properties when exposed to humid conditions. It also limits nanocellulose use in many applications where water is present. This study reveals hydrophobic modification of cellulose nanofiber (CNF) films with vinyl esters of variable alkyl chain length using deep eutectic solvent (DES) of imidazole and triethylmethylammonium chloride as a reaction medium. Additionally, the influence of ultraviolet-ozone (UV/O₃) pretreatment on CNF film modification in DES was addressed. The esterification of CNF films in DES was proven to be a simple and fast approach to increase the hydrophobicity of the films (increasing the contact angle from 38° to 107°), requiring only a 15 min reaction time and reaction temperature of 80 °C. Moreover, the modification improved water vapor barrier properties of the films and resulted in improved mechanical properties at wet state, especially with films treated with UV and ozone before modification.